Skip to main content
. 2021 Jul 12;11(7):1018. doi: 10.3390/biom11071018

Table 2.

Statistical analysis using a 2 tailed t-test of the angular dependence of the modulus of skin (Figure 4). The 0° angle defined as the angle where the maximum modulus is measured. Only the moduli at 0° and 67.5° at 5% strain are significantly different than that of the unstretched skin.

Condition Average Modulus Value Standard Deviation Sample Size p Value Significance
Control (No strain) 2.34 × 106 6.91 × 105 17 NA NA
Strain Direction: 0 degree
(5 Percent Strain)
3.55 × 106 2.56 × 105 5 1.88 × 10−4 * Significant
Strain direction: 67.5 degree
(5 Percent Strain)
3.03 × 106 4.07 × 105 6 1.31 × 10−2 * Significant
Strain direction along 22.5, 45, 90, −67.5, −45, −22.5 degrees
(5 Percent strain)
2.54 × 106 3.12 × 105 27 1.56 × 10−1 Not Significant

* Significantly Different to value at control (No Strain).