Skip to main content
. Author manuscript; available in PMC: 2022 Mar 1.
Published in final edited form as: Addit Manuf. 2021 Jan 26;39:101870. doi: 10.1016/j.addma.2021.101870

Table 1.

Parametric values for print conditions.

Parameters Value Significance
Target Bed Temperature 27–30 ºC Goal temperature of build bed which is adjusted through the emitter lamp.
Binder Set Time 2 sec Amount of time to set binder before drying.
Drying Time 10 sec Amount of time set aside for drying between layers.
Emitter Output 100% The output of the emitter lamp during the drying cycle.
Recoat Speed Varies Speed of the recoater during powder deposition.
Ultrasonic Intensity 100% Strength of ultrasonic attached to the recoater.
Roller Traverse Speed 5 mm/sec Speed of the roller as it goes across the build bed.
Roller Rotation Speed 300 rpm Rate of rotation of the roller.