Skip to main content
. 2021 Jul 23;12:4510. doi: 10.1038/s41467-021-24761-x

Fig. 2. LEC performance as a function of ink solvent, ink storage and ink depostion method.

Fig. 2

The temporal evolution of the luminance and the voltage for LECs fabricated from inks based on chlorobenzene (solid red circles), ethoxybenzene (open blue squares) and anisole (open green diamonds). a The performance of LECs fabricated by spin coating “fresh” inks (prepared the same day). b The performance of LECs fabricated by spin coating “old” inks, which had been stored for 30 days following ink preparation. c The performance of LEC fabricated by scalable bar coating. All devices were driven by a constant current density of j = 77 A m−2.