Table 1.
Parameter | Material | SRA Type | Mixing Temperature | Curing Type and Starting Time 1 | |
---|---|---|---|---|---|
Temperature | UHPC-F4% | None | 10 °C | RH50% | 0 h after casting |
20 °C | |||||
30 °C | |||||
Humidity | UHPC-F3% | None | 30 °C | RH50% | 0 h after casting |
RH100% | 0, 9 or 21 h after casting | ||||
Immersed | 0, 9 or 21 h after casting | ||||
SRA | UHPC-F3% | SRA1—2% | 30 °C | RH50% | 0 h after casting |
SRA2—2% |
1 Characteristics of the first 7 days of curing, afterwards curing at RH50%.