Skip to main content
. 2021 Jul 6;14(14):3786. doi: 10.3390/ma14143786

Figure 16.

Figure 16

Figure 16

Stiffness degradation in sample: (a) SW-26-C-0-R-xx; (b) SW-44-C-0-R-xx; (c) SW-62-C-0-R-xx; (d) DW-26-C-0-R-xx; (e) DW-44-C-0-R-xx; (f) DW-62-C-0-R-xx. Here xx is a crush level (0%; 10%, 20%, and 30%).