FE-SEM images showing the porosity of the sonocoated PEEK substrate in the nanometer range. (A) GoHAP1 for two iterations, (B) three iterations, and (C) five iterations. (D) GoHAP3 for two iterations, (E) three iterations and (F) five iterations. The green line shows the pore in the coating.