Temporal evolution of the median particle size d50 during the wet milling of fenofibrate with CPS beads and fitting of the data by various kinetic models: (a) ω = 3000 rpm and c = 0.35, (b) ω = 3000 rpm and c = 0.5, (c) ω = 4000 rpm and c = 0.35, and (d) ω = 4000 rpm and c = 0.5.