Figure 4.
Microgaphs of metallocene polyethylenes and ultra-high molecular weight polyethylene blends of extrudates obtained at 169 °C. Adequate blend composition brings about smooth extrudates (bottom). The line in the picture corresponds to 1 mm [18] Reprinted with permission from [18]. Copyright 2004 American Chemical Society.