Skip to main content
. 2021 Jul 17;13(14):2348. doi: 10.3390/polym13142348

Table 2.

Calculated linear attenuation coefficients (cm−1) for biodegradable implant materials (magnesium and hydroxyapatite), titanium, cortical bone and skeletal muscle from to 5 to 150 keV. Values can vary depending on structure and density.

Photon Energy (keV) Mg Ti Hydroxyapatite Cortical Bone Skeletal Muscle
5 273.21 3073.09 967.20 350.59 44.08
6 161.41 1941.18 593.03 213.70 25.47
7.112 15.23
7.112 15.25
8 69.36 906.61 270.07 96.65 10.67
9.659 56.85 6.03
9.659 56.89 6.04
10 35.70 494.76 144.49 51.53 5.44
15 10.55 159.02 45.20 16.10 1.65
20 4.48 69.62 19.59 7.03 0.78
30 1.44 21.42 6.11 2.29 0.35
40 0.74 9.35 2.81 1.13 0.25
50 0.50 5.04 1.65 0.72 0.22
60 0.39 3.14 1.13 0.54 0.20
80 0.31 1.63 0.73 0.39 0.18
100 0.27 1.10 0.58 0.34 0.17
120 0.25 0.86 0.50 0.31 0.16
140 0.24 0.73 0.46 0.28 0.16
150 0.23 0.68 0.44 0.28 0.15