. 2021 Jun 18;23(29):15492–15502. doi: 10.1039/d1cp01074c

Fig. 5. (a) LSVs recorded on a GC disk electrode ( = 5 mm) for DME containing 10 mmol dm−3 of GaCl3 and 0.2 mol dm−3 of [TBA][ClO4] at various rotation rates, at a scan rate of 10 mV s−1, at 26 °C. (b) Levich plot constructed using the limiting current densities of the LSVs at −3.0 V vs. Fc+/Fc.

Fig. 5