Figure 8:
Hydrogel characterization. Gel polymerization over time (2% strain and 1 rad/sec) showing Gā (light grey) and Gā (darker grey) with increase of linear acrylamide concentration A) 2.5% and B) 3.37%.
Hydrogel characterization. Gel polymerization over time (2% strain and 1 rad/sec) showing Gā (light grey) and Gā (darker grey) with increase of linear acrylamide concentration A) 2.5% and B) 3.37%.