Skip to main content
. 2021 Jul 27;16:5053–5064. doi: 10.2147/IJN.S311718

Figure 1.

Figure 1

TEM images of (A) NPs and (B) NPs-CUR. (C) Hydrodynamic diameter distribution of NPs and NPs-CUR. Variation of the diameter distribution (D) and TEM image (E) of NPs treated with 100 mM H2O2 for 24 h. (F) Proposed degradation mechanism of mPEG-b-P(PA-alt-GPBAe) by H2O2 and the oxidation products involved.