Table 1. Experimentally and Theoretically Obtained Parameters, i.e., the Bowing Parameter and the Linear Coefficient, Describing Tungsten Content Dependencies of Transition Energies Determined for the Mo1–xWxSe2 Alloy.
| experiment |
theory |
|||
|---|---|---|---|---|
| transition | b [eV] | a [meV/%] | b [eV] | a [meV/%] |
| AML | 0.15 ± 0.04 | |||
| I | 0.001 ± 0.002 | 0.90 ± 0.10 | 0.059 ± 0.050 | 0.20 ± 0.23 |
| A | 0.13 ± 0.03 | 0.25 ± 0.10 | ||
| AH | 0.21 ± 0.10 | |||
| B | 0.14 ± 0.03 | 0.22 ± 0.10 | ||
| BH | 0.19 ± 0.10 | |||
| C | 0.044 ± 0.008 | 0.94 ± 0.10 | 0.22 ± 0.15 | 0.85 ± 0.35 |
| D | 0.010 ± 0.008 | 3.15 ± 0.33 | 0.19 ± 0.15 | 3.21 ± 0.33 |