Skip to main content
. 1994 Mar-Apr;99(2):169–189. doi: 10.6028/jres.099.014

Fig. 12.

Fig. 12

Double logarithmic representation of ate vs te for an epoxy glass aged at Tg −13.2°C. Symbols represent results from tests in which aging response was “probed” at different levels of applied stress: (□) 1 MPa; (○) 5 MPa; (Δ) 10 MPa; (◊) 15 MPa; (●) 20 MPa. (After Ref. [14b].)