Table 1.
Properties of CZA-L and CZA-H catalysts.
| Catalyst | XRD dCuO (nm)a | Surface areab (m2/g) | Pore volumec (cm3/g) | Pore size (nm) | Total Basicity (μmol CO2/g) |
|---|---|---|---|---|---|
| CZA-L | 4.9 | 49.5 | 0.3 | 16.9 | 88.9 |
| CZA-H | 8.7 | 77.5 | 0.5 | 17.4 | 77.3 |
dCuO was determined by the XRD data based on Scherrer's equation.
Surface area was determined by BET method.
Pore volume and pore size were determined by BJH desorption method.