Skip to main content
. 2021 Jul 28;14(15):4227. doi: 10.3390/ma14154227

Figure 5.

Figure 5

The compressive strength of the scaffolds (A) TCP-1, TCP-2, TCP/P(3HB) and (B) SEM microphotograph of TCP/P(3HB) after compressive test. Arrows indicate polymeric microfilaments connecting ceramics’ cracks. Statistically significant differences were indicated by * p ≤ 0.01.