The mass change of the hemp fiber following pretreatment/treatment.

Treatment Weight Change %
Water −4.0 ± 0.3
Alkali treatments −14.2 ± 0.8
Silane modification of water pre-treated fibers −3.0 ± 0.6
Silane modification of alkali pre-treated fibers +0.9 ± 0.0