Experimental conditions used to prepare the physical GE/TN-GO-MB hydrogels, as well as the MB concentration incorporated in the hydrogels.

Condition Hydrogel GO
(% wt/wt)
GE + TN + GO + MB
(mg) a
MB Concentration b
(mg/mL)
01 1-GE/TN-GO-MB 0.31 67.86 0.13
02 2-GE/TN-GO-MB 0.51 68.01 0.13
03
04
3-GE/TN-GO-MB
4-GE/TN-GO-MB
0.71
1.02
68.14
68.35
0.13
0.13