Figure 11.

Figure 11

Mud cake thickness attained using (a) CMC, (b) 1:6, (c) 1:4, and (d) 1:3 Fe3O4-CMC nanocomposite ratios. The mud cake thickness was reduced by 44.27%, 51.14%, and 64.88%, respectively, as compared to CMC, which showed an increase in thickness of up to 48% [107].