Skip to main content
. 2021 Jul 29;13(15):2502. doi: 10.3390/polym13152502

Figure 2.

Figure 2

Evolution of number-average molar mass (Mn, black squares) and dispersity (Đ, red open circles) with conversion for the RAFT dispersion polymerization of HFBMA at 10% w/w solids in ethanol at 70 °C using a PDMA39 macro-CTA with macro-CTA/AIBN molar ratio of 5/1. The targeted diblock composition was PDMA39–PHFBMA200.