Skip to main content
. 2021 Jul 24;13(15):2439. doi: 10.3390/polym13152439

Table 1.

Average, median and standard deviations for hydrophobicity measurement of pure PVDF fibers and PVDF with Ca(NO3)2, Mg(NO3)2 and Zn(NO3)2.

Average/° Median/° Std. Dev./° Std. Dev./%
PVDF 127.1 127.6 7.6 6.0
PVDF with Ca(NO3)2 124.1 125.2 11.9 9.6
PVDF with Mg(NO3)2 131.3 131.4 4.6 3.5
PVDF with Zn(NO3)2 135.9 135.9 7.8 5.8