Table 4.
Different parameters used for the manufacturing of the leg splint.
| Layer height [mm] | 0.2 |
| Extruder [mm] | 0.4 |
| Density [%] | 40 |
| Thickness perimeter each layer [mm] | 1 |
| Print speed [mm/s] | 60 |
| Temperature [°C] | 220 |
Different parameters used for the manufacturing of the leg splint.
| Layer height [mm] | 0.2 |
| Extruder [mm] | 0.4 |
| Density [%] | 40 |
| Thickness perimeter each layer [mm] | 1 |
| Print speed [mm/s] | 60 |
| Temperature [°C] | 220 |