Skip to main content
. 2021 Jul 30;9(8):83. doi: 10.3390/dj9080083

Figure 6.

Figure 6

The topography changes of the bulk-fill (BF) composites cured in different conditions. (A) The mean and standard deviation of ΔRa values considering the underperformed light curing conditions and the two-radiance emittance output (mean ± sd; n = 6). Capital letters compare LCU600, while lower case letters compare LCU1000. Dissimilar letters are significantly different from each other (p < 0.05). (BE) Representative SEM images of the BF composite surface under control and moderate angulation following the output of 1000 mW/cm2 (B,C) and LCU600 (D,E).