Experimental values of the Mössbauer spectra of Fe3O4 nanoparticles at different stages of modification and carboranes immobilization.

Sample A-Sublattice
Hn, kOe
B-Sublattice
Hn, kOe
Intensity of Doublet, % IB-sublattice/IA-sublattice δ (Fe3-δ)O4 χ2
Fe3O4 475.34 ± 3.24 425.84 ± 4.53 0.7 74.9/24.4 0.327 ± 0.031 0.94 ± 0.03
Fe3O4-TMSPM 479.57 ± 2.32 427.07 ± 3.43 0.6 75.8/23.6 0.331 ± 0.025 1.09 ± 0.05
Fe3O4-TMSPM-PAA 469.42 ± 3.25 422.65 ± 4.31 1.2 84.5/14.3 0.330 ± 0.027 1.10 ± 0.06
Fe3O4-TMSPM-PAA/PALAm 465.75 ± 4.21 440.54 ± 3.64 2.5 87.4/10.1 0.332 ± 0.025 1.08 ± 0.04
Fe3O4-TMSPM-PAA/PALAm-Gd 465.32 ± 4.14 435.17 ± 5.42 1.6 86.5/11.9 0.322 ± 0.016 1.04 ± 0.10
Fe3O4-TMSPM-PAA/PALAm-Gd -PAA 459.65 ± 3.52 437.13 ± 2.31 1.1 87.2/11.7 0.304 ± 0.014 1.01 ± 0.09
Fe3O4-TMSPM-PAA/PALAm-Gd- PAA/PALAm 469.64 ± 2.45 435.65 ± 2.56 0.9 87.7/11.4 0.323 ± 0.021 1.05 ± 0.07
Fe3O4-TMSPM-PAA/PALAm-Gd- PAA/PALAm—Carborane 468.42 ± 2.63 437.39 ± 2.35 0.7 86.2/13.1 0.317 ± 0.027 1.21 ± 0.04