Skip to main content
. 2021 Aug 4;13(16):2582. doi: 10.3390/polym13162582

Figure 6.

Figure 6

SEM micrographs, at different magnifications, of cPLA, cPLA-BP and cPLA-L fibres after immersion in water for 7 days. Scale bars: 5 µm (left hand side), 10 µm (right hand side).