. 2021 Aug 16;14(16):4605. doi: 10.3390/ma14164605

Table 2.

Material FPP parameters and exposure energy dose required to achieve a full conversion ratio during the printing process according to the reinforcement solid load content.

SL 0% SL 5% SL 10% SL 15%
μ (mm−1) 1.139 2.45 3.69 4.59
K(cm2/mJ) 0.0045 0.0073 0.0094 0.0107
d0 (mJ/cm2) 126 227 252 277