Skip to main content
. 2021 Aug 19;13(16):2785. doi: 10.3390/polym13162785

Figure 4.

Figure 4

Figure 4

Degradation of films after the third and fourth month: (a) B0 after 3 months, (b) B0 after 4 months, (c) SP after 3 months, (d) SP after 4 months, (e) SW after 3 months, (f) SW after 4 months, (g) B1 after 3 months, (h) B1 after 4 months, (i) B2 after 3 months, (j) B2 after 4 months, (k) Eco after 3 months, (l) Eco after 4 months, (m) K after 3 months, (n) K after 4 months. The figure shows all 7 films only after the third and the fourth month because in most cases after the first and even after the second month no change and decomposition was visually observed.