Skip to main content
. 2021 Aug 23;13(16):2832. doi: 10.3390/polym13162832

Figure 6.

Figure 6

Figure 6

Thermal shrinkage of HDPE/EVA/PU blends: (a) reduction rate of non-irradiated sample and samples irradiated at 75 kGy and 150 °C for 1 h, (b) reduction rate of non-irradiated sample and samples irradiated at 75 kGy and 180 °C for 1 h, and (c) optical images of the HDPE/EVA/PU blends with non-irradiated and samples irradiated at 23 °C and 180 °C for 1 h.