Skip to main content
. 2021 Aug 6;14(16):4414. doi: 10.3390/ma14164414

Figure 1.

Figure 1

X-ray diffraction patterns for TiO2 sintered at different temperatures (700, 800, 900, and 1000 °C). Diffraction patterns for anatase and rutile TiO2 are based on PDF of ICDD.