Figure 2.

Figure 2

SEM images: (A) Unsintered TiO2; (B) TiO2 sintered at 700 °C; (C) TiO2 sintered at 800 °C; (D) TiO2 sintered at 900 °C; (E) TiO2 sintered at 1000 °C; (F) Control (Celldesk LF1, Polystyrene film dish). Scale bar = 5 μm for all the images.