Figure 4.
Effect of polypropylene (PP) content (hollow markers) and melt mass-flow rate (MFR, solid markers) on the (a) tensile modulus (), (b) elongation at break ( ) and (c) tensile impact strength ( ) of PE-LD and mixed PO regranulates. Effect of 5 wt.% ethylene-based olefin block copolymer on the (d) , (e) and (f) of PE-LD and mixed PO regranulates (solid markers prior to compatibilisation and hollow markers after).