Table 5.

Mean flexural strength and toughness parameters of FRGM with hybrid fibres.

Parameters ARG0.5-S0.5 PVA1.0-S0.5 PVA1.0-ARG0.5 PP1.0-S0.5 PP1.0-ARG0.5
First crack strength (MPa) 4.56 4.02 4.89 5.67 4.7
Flexural strength (MPa) 5.29 4.7 4.89 5.69 4.7
Standard deviation flexural strength 0.45 0.38 0.35 0.28 0.31
Toughness indices I5 5.06 4.95 4.28 3.94 2.74
I10 10.61 10.38 8.6 7.8 4.37
I20 21.7 21.35 16.52 15.4 6.65
Residual strength factors R5,10 111 108.44 86.47 77.14 32.66
R10,20 110.98 109.7 79.21 76.04 22.74