(A) Specific capacity for a PBA electrode fabricated with conventional WPI at different degrees of calendering at different C-rates. (B) Capacities of uncalendered electrodes fabricated with conventional WPI and fabricated with WPI using an immersion bath at 85 °C and pH 12. All cycling experiments were performed in a 1 M NaCl flooded cell.