Skip to main content
. 2021 Jul 6;121(17):10241–10270. doi: 10.1021/acs.chemrev.1c00148

Figure 2.

Figure 2

Scanning electron micrograph (left, a) and photograph (right, b) after polarization of a tin cathode at 175 mA cm–2 in 0.5 M KHCO3 at 500 and 3000 rpm, respectively. Reproduced with permission from ref (78). Copyright 2011, Springer Science Business Media BV.