Skip to main content
. 2021 Aug 26;14(17):4854. doi: 10.3390/ma14174854

Figure 5.

Figure 5

Comparison of the experimental results (points) and simulation (line) (a), as well as the distribution of the relative thickness of the LiNbO3 film on a substrate with a diameter of 100 mm (b).