Material Geometry Tensile Test [cm3] Standard Amplitude [μm] Time [s] Pressure/Velocity Ref.
PLA 1.5 × 0.1 × 0.1 IRAM-IAS-U500-102/3 48.1 3 3 bar [112]
PLA Poly (nonamethylene azelate)
(PE99)
1.5 × 0.1 × 0.1 IRAM-IAS-U500-102/3 24 1.2 300 N [121]
PA12 33 × 2.5 × 1.25 ASTMD638 35 5 2 bar [108]
Poly (ε-caprolactone) Graphistrength® C10 carbon nanotubes 1.5 × 0.1 × 0.1 IRAM-IAS-U500-102/3 37 7 or 8 2500 N [139]
PEEK 30 × 2 × 2 ASTMD638 52.2/58 8/5 5/6 [117]
PPSU 30 × 2 × 2 ASTMD638 58/40.6 1.4/2.8 11/5 [113]
UHMWPE 30 × 2 × 1 ISO-527-4 50.6/56.2 [106]
UHMWPE + graphite [114]