Figure 5.

Figure 5

The mass loss per oxide surface area, mdiss (ac) for 15, 100, and 200 mA·cm−2, respectively, and current density of Al dissolution, obtained from dissolved Al3+ (df) for 15, 100, and 200 mA·cm−2, respectively, as a function of arsenazo-I concentration for Al in 0.6 M malonic acid.