Skip to main content
. 2021 Sep 6;14(17):5118. doi: 10.3390/ma14175118

Figure 6.

Figure 6

(a) Volume expansion factor, as a function of arsenazo-I concentration for Al in 0.6 M malonic acid; FTIR-spectroscopy: malonic acid without arsenazo-I, ja = 15, 78, 134, 200 mA·cm−2 (dashed lines); (b) malonic acid with 3 g·L−1 arsenazo-I, ja = 15, 100, 200 mA·cm−2 (solid lines).