Skip to main content
. 2021 Sep 6;14(17):5118. doi: 10.3390/ma14175118

Figure 10.

Figure 10

(a) XRD spectra of the initial aluminum foil (curve 2) and a glass substrate with an adhesive layer applied to foil (curve 1). (b) XRD spectra of porous aluminum oxide film samples obtained in 0.6 M malonic acid without additive at current densities 2.54, 60.7, 150 and 243 mA·cm−2 (curves 1, 2, 3 and 4 respectively). (c) XRD spectra of porous aluminum oxide film samples obtained in 0.6 M malonic acid with an addition of arsenazo-I 3.24 g·L−1 and a current density of 15 mA·cm−2 (curve 1), and 2.50 g·L−1 and a current density of 200 mA·cm−2 (curve 2).