Figure 11.

Figure 11

Dependence the XRD peak intensity of aluminum on the anodic current density during galvanostatic anodizing in pure 0.6 M MA in the 2Θ ranges of (a) 37.7–39.1°, (b) 63.5–67.5°, and (c) 77.5–79.1°.