Skip to main content
. 2021 Aug 27;13(17):2883. doi: 10.3390/polym13172883

Figure 7.

Figure 7

(a) Galvanostatic charge-discharge plots and (b) specific capacitance as a function of current density, and (c) EIS; Inset: EIS of Pbp@HD between 100 kHz and 40 mHz, and (d) electrochemical equivalent circuit (CPE = constant phase element, Ws = short Warburg Diffusion).