Skip to main content
. 2021 Sep 2;14(17):5017. doi: 10.3390/ma14175017

Figure 4.

Figure 4

Distribution of Ni/CeO2 active phase (white) on the surface of carbon (grey) monoliths prepared with different R/W molar ratio for conventional design (AC) and R/W = 17 for tortuous design (D). Left: Monolith transversal section, center: Monolith longitudinal section and Right: Inside channel wall.