Summary of the SiPM specification whose secondary photon emission is studied in this work [2,6]. The Fill Factor is defined as the ratio between the photon-sensitive area to the total area of the SiPM. The breakdown voltages are extracted from the SiPM I-V curves; defined as the voltage for which the first derivative with respect to the voltage of the SiPM current (in log space) is at the maximum [23].

Parameter FBK VUV-HD3 HPK VUV4
Total Area 6 × 6 mm2 3 × 3 mm2
SiPM Fill Factor 80% 60%
SPAD pitch 35×35μm2 50×50μm2
Breakdown Voltage [298 K] 31 ± 1 V 52 ± 1 V