. 2021 Sep 3;6(36):23564–23569. doi: 10.1021/acsomega.1c03687

Table 2. Peak Temperatures of Hydrogen Desorption and the Amount of Absorbed Hydrogen on the Prepared MgH2 with Each Nb2O5.

name peak temperature of H2 desorption (°C) amount of absorbed H2 (wt %)
mono-NbO 247, 283 (36) 1.7
amor-NbO 242, 273 (31) 2.2
pyro-NbO 242, 253 (11) 3.7
layered-NbO 237, 259 (22) 3.0
ortho-NbO 232, 262 (30) 2.7