Skip to main content
. 2021 Sep 2;14(17):5020. doi: 10.3390/ma14175020

Figure A5.

Figure A5

The Mössbauer spectra obtained at 296 K of ZPR roasted: (a) without additions at 600 °C; (b) with addition of 48% Fe2(SO4)3 at 600 °C, then additionally calcined at 900 °C; (c) with addition of 48% Fe2(SO4)3 at 600 °C, water-leached, then additionally calcined at 900 °C.