Skip to main content
. 2021 Sep 18;14(18):5404. doi: 10.3390/ma14185404

Figure 2.

Figure 2

Selected features of MZ + 0.0Sn alloy microstructure after DSC measurement: (a) example of ternary eutectic; (b) example of binary eutectic; (c) example of Mg2Zn11 and MgZn2 mixture; (d) area with EDS measurement points 1–4 listed in Table 2.