Skip to main content
. 2021 Sep 10;13(18):3064. doi: 10.3390/polym13183064

Figure 13.

Figure 13

(a) Normalized ECSA until 30,000 cycles of the AST durability test in N2-saturated 0.1 M HClO4 of Pt/C-S, Pt/C, and C-Pt/C. ORR polarization curve before and after 30,000 cycles of AST of (b) Pt/C-S, (c) Pt/C, and (d) C-Pt/C. Numbers in (bd) indicate the initial and final cycle of the AST durability test. Reproduced with permission from Elsevier (reference [235]).