. 2021 Sep 14;14(18):5290. doi: 10.3390/ma14185290

Figure 4.

Figure 4

BSEM images indicating the extend of IG corrosion observed for the as-cast samples after 1000 h of NSST: (a) MZ + 0.0Sn (b) MZ + 0.5Sn (c) MZ + 3.0Sn.