Skip to main content
. 2021 Sep 14;14(18):5290. doi: 10.3390/ma14185290

Figure 9.

Figure 9

MZ + 2.0Sn annealed microstructure after 1000 h in NSST affected by IG corrosion: (a) overview, (b) detail.