Skip to main content
. 2021 Sep 7;11(9):692. doi: 10.3390/membranes11090692

Table 1.

Comparison of the crystallinity degree at 23 °C determined by DSC and WAXS analysis (the standard deviation on Xc values is greater than 2%).

Films Xc,23°C (%) Xc,23°C (%)
DSC WAXS
Pebax® 17 25
P/PEGOH10 13 23
P/PEGOH30 8 20
P/PEGOH50 6 18
P/PEGDME10 14 22
P/PEGDME30 10 18
P/PEGDME50 7 15
P/PEGOH5/PEGDME5 14 25
P/PEGOH15/PEGDME15 8 18
P/PEGOH25/PEGDME25 6 16
P/PEGOH3.75/PEGDME6.25 12 23
P/PEGOH11.25/PEGDME18.75 8 21
P/PEGOH18.75/PEGDME31.25 6 16